Showing posts with label Tellurium. Show all posts
Showing posts with label Tellurium. Show all posts

Tellurium

Table 1.  Te 3d5/2 binding energy values [1].
Te 3d5/2 - 3d3/2 splitting: 10.39 eV [2]
Te 3p3/2: 820 eV
Te 3p1/2: 871 eV
Te 3s: 1009 eV
Te 5s: 12 eV
Te 4d5/2: 41 eV
Te 4d3/2: 42 eV
Te 4p: 111 eV
Te 4s 170 eV

O 1s for TeO2: 530.4 eV +/- 0.2 eV
R.S.F. Te 3d = 9.508, Te 3d5/2 = 5.705

Te 3d5/2 - M4N45N45 Auger parameter values [1].

References:
[1] C.D. Wagner, A.V. Naumkin, A. Kraut-Vass, J.W. Allison, C.J. Powell, J.R.Jr. Rumble, NIST Standard Reference Database 20, Version 3.4 (web version) (http:/srdata.nist.gov/xps/) 2003.
[2] J.F. Moulder, W.F. Stickle, P.E. Sobol, K.D. Bomben, Handbook of X-ray Photoelectron Spectroscopy, Perkin-Elmer Corp., Eden Prairie, MN, 1992.