Showing posts with label Iodine. Show all posts
Showing posts with label Iodine. Show all posts

Iodine

I 3d5/2 binding energies.
Notes:
I 3d5/2-3/2 Splitting = 11.50 eV

I 3p3/2: 875 eV
I 3p1/2: 930 eV
I 3s: 1071 eV
I 4d5/2: 49 eV
I 4d3/2: 51 eV
I 4p: 123 eV
I 4s: 187 eV
I 5s: 18 eV

I 3d R.S.F. (Kratos) = 10.343
I 3d5/2 R.S.F. = 6.2058