Showing posts with label Caesium. Show all posts
Showing posts with label Caesium. Show all posts

Caesium

 

Cs 3d5/2 binding energy values.

Note: Cs 3d5/2 - 3d3/2 splitting is 13.94 eV

Cs 3s: 1219 eV

Cs 3p3/2: 1002 eV

Cs 3p1/2: 1069 eV

Cs 4s: 234 eV

Cs 4p3/2: 161 eV

Cs 4p1/2: 173 eV

Cs 4d5/2: 77 eV

Cs 4d3/2: 80 eV

Cs 5s: 25 eV

Cs M5N45N45: 931 eV (Al)

Cs M4N45N45: 918 eV (Al)