Reference:
[1] J.J. Yeh, Atomic Calculation of Photoionization Cross-Sections and Asymmetry Parameters, Gordon and Breach Science Publishers, Langhorne, PE (USA), 1993.
[2] J.J. Yeh and I.Lindau, Atomic Data and Nuclear Data Tables 32 (1985) 1-155.
X-ray photoelectron spectroscopy (XPS or ESCA) curve fitting procedures, reference materials and useful notes are listed here to provide a starting point for the consistent interpretation of XPS spectra. These reference pages contain tips and techniques that are designed to help both the novice and advanced XPS user.