Peter Sherwood at the University of Washington has recently published a very good review article [1] that goes through many of the issues and pitfalls associated with achieving meaningful results from curve fitting XPS spectra. It also includes a useful tutorial section that uses the W 4f spectrum of oxidized tungsten to illustrate the methods outlined in the paper. A good starting point read for those who are getting into curve-fitting of XPS spectra (and for those needing a refresher!).
Reference:
[1] Peter M.A. Sherwood, The use and misuse of curve fitting in the analysis of core X‐ray photoelectron spectroscopic data, Surf. Interface Anal. 51 (2019) 589-610.