| Tin Auger (Sn 3d5/2 - M4N45N45) parameter values [1,2,3,4]. |
Sn Auger spectra are available from [6].
References:
[1] C.D. Wagner, A.V. Naumkin, A. Kraut-Vass, J.W. Allison, C.J. Powell, J.R.Jr. Rumble, NIST Standard Reference Database 20, Version 3.4 (web version) (http:/srdata.nist.gov/xps/) 2003.
[2] L. Kover, G. Moretti, Zs. Kovacs, R. Sanjines, I. Cserny, G. Margaritondo, J. Palinkas, H. Adachi, J. Vac. Sci. Technol. A. 13 (1995) 1382-1388.
[3] L. Kover, Zs. Kovacs, R. Sanjines, G. Moretti, I. Cserny, G. Margaritondo, J. Palinkas, H. Adachi, Surf. Interface. Anal. 23 (1995) 461-466.
[4] K. Schenk-Meuser, H. Duschner, Fresenius J. Anal. Chem. 358 (1997) 265-267.
[5] V.M. Jimenez, J.P. Espinos, A.R. Gonzalez-Elipe, Surface Science 366 (1996) 556-563.
[6] S. Suzer, Pure & Appl. Chem. 69 (1997) 163-168.