Figure 1. Shake-up structure in Cu 2p spectra of copper (II) hydroxide (Cu(OH)2, top) and copper (II) oxide (CuO, bottom)[2].
Figure 2. Cu 2p spectra of various Cu(II) species[3].
References:
[1] F. de Groot, A. Kotani “Core Level Spectroscopy of Solids” CRC Press, Boca Raton, 2008, p 147.
[2] M.C. Biesinger, L.W.M. Lau, A.R. Gerson, R.St.C. Smart, Appl. Surf. Sci. 257 (2010) 887.
[3] M.C. Biesinger, Surf. Interface Anal. 49 (2017) 1325.
[1] F. de Groot, A. Kotani “Core Level Spectroscopy of Solids” CRC Press, Boca Raton, 2008, p 147.
[2] M.C. Biesinger, L.W.M. Lau, A.R. Gerson, R.St.C. Smart, Appl. Surf. Sci. 257 (2010) 887.
[3] M.C. Biesinger, Surf. Interface Anal. 49 (2017) 1325.
2.jpg)