X-ray photoelectron spectroscopy (XPS or ESCA) curve fitting procedures, reference materials and useful notes are listed here to provide a starting point for the consistent interpretation of XPS spectra. These reference pages contain tips and techniques that are designed to help both the novice and advanced XPS user.
Pages
▼
Fluorine
F 1s binding energy values.
Notes: [1] lists -CH2CHFCH2- (PVF) at 686.94 eV, (-CF2-CF2-)n (PTFE) at 689.67 eV, and OOCCF3 (PVTFA) at 688.16 eV.
F 2s: 30 eV
Reference:
[1] G. Beamson, D. Briggs, High Resolution XPS of Organic Polymers - The Scienta ESCA300 Database Wiley Interscience, 1992.