Pages

▼

More Molybdenum Values

Table 1. Average Mo 3d5/2 binding energy values from a compilation of literature sources [1].

Reference:
[1] C.D. Wagner, A.V. Naumkin, A. Kraut-Vass, J.W. Allison, C.J. Powell, J.R.Jr. Rumble, NIST Standard Reference Database 20, Version 3.4 (web version) (http:/srdata.nist.gov/xps/) 2003.