Pages

▼

Indium 3d5/2 - M4N45N45 Auger Parameter

Indium MNN Auger spectrum.  The In M4N45N45 peak is shown with a peak fit to it. This is the more common peak to use for the calculation of the Auger parameter.
Note that the In M4N45N45 peak is the more common peak to use for the calculation of the Auger parameter.

In 3d5/2 - M4N45N45 Auger Parameter Values [1]

Reference:
[1] C.D. Wagner, A.V. Naumkin, A. Kraut-Vass, J.W. Allison, C.J. Powell, J.R.Jr. Rumble, NIST Standard Reference Database 20, Version 3.4 (web version) (http:/srdata.nist.gov/xps/) 2003.