Pages

Indium

In 3d5/2 binding energy values [1].
In 3d5/2 - 3d3/2 splitting is 7.54 eV [1]
In 3p3/2: 605 eV
In 3p1/2: 703 eV
In 3s: 828 eV
In 4d: 17 eV
In 4p: 78 eV
In 4s: 123 eV

In 3d spectrum of an argon ion sputter cleaned indium metal surface.
In 3d5/2 peakshape for indium metal is LA(1.1,1.7,3), FWHM 0.53 eV (20 eV pass energy).

Reference:
[1] C.D. Wagner, A.V. Naumkin, A. Kraut-Vass, J.W. Allison, C.J. Powell, J.R.Jr. Rumble, NIST Standard Reference Database 20, Version 3.4 (web version) (http:/srdata.nist.gov/xps/) 2003.