Pages

▼

Common O 1s Values


Table 1. A series of common O 1s binding energy values.

From reference [1] it is found that oxygen bound to organic components can range in binding energy from as low as 530.9 eV to as high as 533.8 eV (corrected here to C 1s (C-C, C-H) at 284.8 eV).  The more common organic oxygen species (alcohols, esters, ketones, ethers and organic acids) are found in a range from 532.0 - 533.7 eV. This post shows a very handy table of organic oxygen species.
Reference:
[1] G. Beamson, D. Briggs, High Resolution XPS of Organic Polymers - The Scienta ESCA300 Database Wiley Interscience, 1992.